MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Latene® EP 7UV-V Polypropylene Copolymer (PPC) (UL94 V-2)  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Description: Latene EP thermoplastics are polypropylene copolymer (PPC) products. They are distinguished by their resistance to low temperatures and good chemical inertness. Filled EP Latenes have rigidity, shrinkage and good surface finish. UV-stabilized versions may be supplied, giving products with good weathering resistance. Latene is used especially in garden furniture. Heat-stabilized, anti-static versions are possible.

Specific Notes for this Material: UL94V-2 self-extinguishing, with halogens; class 1 in compliance with CSE RF 2/75/A and CSE RF 3/77; UV-stabilized; high flowability; excellent surface finish; specific for seats and benches for public areas.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Water Absorption 0.020 %0.020 %at 23°C; ISO 62
Linear Mold Shrinkage 0.013 cm/cm0.013 in/inLATI
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inLATI
Melt Flow 12 g/10 min12 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5555ASTM D785
Tensile Strength, Ultimate 22.0 MPa3190 psiISO 527
Flexural Modulus 1.19 GPa173 ksiASTM D790
Izod Impact, Notched 0.500 J/cm
@Temperature 23.0 °C
0.937 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
DIN 53453
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
IEC 243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C198 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C129 °FASTM D648
Vicat Softening Point 68.0 °C154 °F50°C/h 50N; ISO 306
Flammability, UL94 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
Glow Wire Test  960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 695-2-1
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 200 °C356 - 392 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 70.0 - 90.0 °C158 - 194 °FTemperature can be reduced when using vacuum ovens.
Dry Time >= 3 hour>= 3 hourDrying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedmedium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLATI115 / 50113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.