MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Duct 821U01 Thermally Conductive Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 821U01 one component, thermally conductive adhesive is designed for such applications as substrate attach, sealing micro-electronic packages, heat sink attach, and component staking. This adhesive provides four (4) strong adhesions to difficult-to-bond metals, such as gold, silver, and copper. It retains its bond strength after exposure to moisture.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 33000 cPMixed (cp #52, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 854 hrs @ 93°C
Adhesive Bond Strength 2200 psiLap shear, alum to alum, 30 min @ 150°C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.670 W/m-K
@Temperature 100 °C
Glass Transition Temp, Tg 115 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 115 °C
 
Descriptive Properties
Color BlackMixed/Cured
Thixotropic Index 1.31 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC166 / 71094

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.