MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.

Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals.

Characteristics of Arnitel:

  • Excellent strength over a wide range of temperatures
  • Excellent dynamic properties e.g. creep and fatigue
  • High heat resistance
  • Exceptional resistance to oils and greases
  • Good chemical resistance
  • High degree of versatility in processing
  • Easy coloring using masterbatches
  • Surface quality from high gloss to textured
  • Excellent heat resistance (long term 165°C)
  • Good electrical insulation properties
  • Low moisture absorption, excellent dimensional stability
  • Easy flow, fast cooling times

Typical Applications:

  • Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
  • Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in consumer electronic companies. Arnitel® is a good choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.

Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs.

Information provided by DSM.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183
Water Absorption 0.60 %Sim. to ISO 62
Moisture Absorption at Equilibrium 0.15 %Humidity Absorption; Sim. to ISO 62
Melt Flow 19.35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Calculated from Volume Flow Rate of 15 cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 723 s; ISO 868
Tensile Strength at Break 38.0 MPaISO 527-1/-2
Tensile Stress at Strain 24.9 MPa
@Strain 50 %
ISO 527-1/-2
 31.2 MPa
@Strain 5.0 %
ISO 527-1/-2
 34.4 MPa
@Strain 10 %
ISO 527-1/-2
Elongation at Break 250 %ISO 527-1/-2
Elongation at Yield 10 %ISO 527-1/-2
Tensile Modulus 1.00 GPaISO 527-1/-2
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 23.0 kV/mmIEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Melting Point 221 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1/-2
Vicat Softening Point 160 °C50°C/h 50N; ISO 306
 210 °C50°C/h 10N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
Glow Wire Ignition Temperature 850 °C
@Thickness 1.00 mm
IEC 60695-2-13
 
Descriptive Properties
High impact or impact modifiedYes
Injection MoldingYes
Without fillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Envalior Arnitel® EL740 TPC-ET, Injection Molding
LyondellBasell Montell SE191 Polypropylene Impact Copolymer
Envalior Arnitel® EL740 Polyether Ester Elastomer (European and Asian Grade)
Covestro Desmopan® 9665DU Polyurethane

PDSMA204 / 31078

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.