MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/760 UV Polyolefin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Cogegum® HFFR -Halogen Free Fire Retardant compound

Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution; furthermore, toxic and corrosive gases emission and smoke generation are particularly reduced. These characteristics make this compound suitable in all applications where the fire behavior of cable materials is one of the main concerns to be considered in establishing a high safety level in public places. This material complies with RoHS requirements.

standard complying

- EN 50363-0 M1; EN 50363-7 TI6, TI7; IEC 60502-1 ST8; Cenelec HD 624.7 S1; Cenelec HD 624.6 S1; VDE 0207 HM2, HM5, HJ2; IEC 60092 SHF1; UNE 21123-4

Flame Retardant; Halogen Free; Low Smoke Emission; Low Toxicity; Self Extinguishing; UV Resistant

Uses: Cable Jacketing; Low Voltage Insulation; Wire & Cable Applications

Availability: Asia Pacific; Europe; North America

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
ESCR 10% Igepal® >= 1000 hourASTM D1693
Melt Flow 3.2 g/10 min
@Load 21.6 kg,
Temperature 150 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51ISO 868
Tensile Strength at Break 12.3 MPaASTM D638
Elongation at Break 190 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.50e+11 ohm-cm
@Temperature 70.0 °C
ASTM D257
 1.10e+14 ohm-cm
@Temperature 20.0 °C
ASTM D257
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 37 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 130 - 150 °C
Zone 2 130 - 160 °C
Zone 3 140 - 160 °C
Zone 4 140 - 160 °C
Die Temperature 150 - 180 °C
 
Descriptive Properties
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/760 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/720-UV Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/710 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/960 Polyolefin
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/920-UV Polyolefin

PSOL8Y6159 / 193080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.