MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Features:
  • High heat resistance
  • Good chemical resistance
  • High impact strength
  • Excellent flow characteristics

Applications:

  • Automotive interior trim applications
  • Automotive consoles
  • Structural Housings

Information provided by Nova Chemicals

INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. 

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccISO 1183
Linear Mold Shrinkage 0.0070 cm/cmISO 2577
Melt Flow 1.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 36.0 MPaISO 527-2
Elongation at Break 16 %ISO 527-2
Tensile Modulus 2.60 GPaISO 527-2
Flexural Strength 69.0 MPaISO 178
Flexural Modulus 2.70 GPaISO 178
Izod Impact, Notched (ISO) 0.660 J/cm²ISO 180/1A
Charpy Impact Unnotched 5.20 J/cm²ISO 179/1eU
Charpy Impact, Notched 0.650 J/cm²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 75.0 µm/m-°C
@Temperature 20.0 °C
NOVA Chemicals Laboratory Procedure
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
@Diameter 4.00 mm
Unannealed; bar; ISO 75-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 - 260 °CProfile temperatures
Melt Temperature 204 - 260 °Cair purge at equilibrium conditions
Mold Temperature 43.0 - 60.0 °CCore surface temp. at equilibrium
 54.0 - 71.0 °CCavity surface temp. at equilibrium
Back Pressure 50.0 - 100 psiTypically 50 psi
Screw Speed 40 - 80 rpm
 
Descriptive Properties
Injection Speedmedium-fastTypically fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer
Ineos Nova 1204 High Heat Crystal Polystyrene
DuPont Teijin Films Mylar® RL42 Polyester Packaging Film, 150 Gauge
DuPont Teijin Films Mylar® RL33 Polyester Packaging Film, 150 Gauge

PNOV950 / 54896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.