System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Karina E 85/201-DA-IS-SI Clear PVC Compound
Categories:
Polymer
;
Film
;
Thermoplastic
;
Vinyl (PVC)
Material Notes:
Non toxic PVC compound, free of phthalate plasticizers, recommended for stretch films for food contact use.
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.22
-
1.28
g/cc
ASTM D 792
Mechanical Properties
Original Value
Comments
Hardness, Shore A
81 - 85
@Time 15.0 sec
ASTM D 2240
Tensile Strength
>=
180
kg(f)/cm²
ASTM D 638
Elongation at Break
>= 150 %
ASTM D 638
Descriptive Properties
Application
General Purpose Films
Clarity
OK
ME 03
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Aurora Plastics GA-7056D-FR-105 PVC
Aurora Plastics TufTech™ GA-3188AHP PVC Compound
Karina 85/201-DA-IS-SI-AT Clear PVC Compound
Karina E 85/201-DA-IS-SI-AT Clear Crystal PVC Compound
Armacell ArmaSport® MFC-2 Continuous Rolls, PVC/NBR
PKARIN9390 / 171046
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.