MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt IMEDGE® PCT110 Polymer Coating Technology
Categories: Polymer; Thermoset

Material Notes: IMEDGE® PCT100 and PCT110 coatings are advanced Polymer Coating Technology (PCT) products that have been formulated to be used as in-mold, exterior coatings for reinforced plastic parts.

Features and Benefits:

  • Deep, dark, rich, high gloss colors
  • Excellent color and gloss recovery after sanding and buffing
  • Exceptional water resistance
  • Excellent blush resistant
  • IMEDGE® PCT100 has excellent weathering resistance
  • IMEDGE® PCT110 has exceptional weathering resistance
  • Enhanced impact resistance and toughness for reduced cracking
  • Excellent scratch and wear resistance
  • Resistant to porosity
  • Low weight per gallon

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 9000 - 13000 cP9000 - 13000 cPRVF, spindle #4 @ 4 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 26.1 - 27.8 °C79.0 - 82.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 - 160 min1.50 - 2.67 hourLay-up Time
Gel Time 12.0 - 20.0 min12.0 - 20.0 min100 g mass, 1.8% MEKP
 
Descriptive Properties
Sag ResistanceGood @ 20 mils
Thixotropic Index4-6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9207 / 231802

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.