MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ND Industries Vibra-Tite® Formula 3
Categories: Polymer; Adhesive; Thermoset

Material Notes: General Description

Engineered to be cost-effective and CFC-free, ND Vibra-Tite Formula 3 is a non-ozone depleting, locking and sealing coating for threaded fasteners. Vibra-Tite utilizes a special blend of acrylic resins to prevent fasteners from loosening-even under extreme vibration.

Designed for use on male and female

Applications

From tiny eyeglass screws to huge construction bolts, vibratite is ideal for use on fasteners of any size. In addition to supplying bottles and cans on Vibra-Tite for "User-Applied," on the job application, fasteners can be "Pre-Applied" at any of ND Industries eight regional service centers.

Meets or exceeds military specification:

  • Mis-28867
  • U.S. Air Force Part # 19207
  • U.S. Army Tank Automotive Command (General Dynamics) Part # 11663357
  • National Stock Number NSN-8030-00-163-5792
OEM Standards:
  • Detroit Diesel 9S244 & 9S256
  • Grumman Aircraft Part # GF-105 CA1
  • Allied Signal Aerospace Company Part # EMS73314
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 165 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
Chemical resistance to Salt WaterTotally ResistantActs as a partial corrosion barrier
Chemical resistance to solventsSome Resistance
Chemical resistance to WaterTotally Resistant
ColorRed (Custom colors available)
Cured Formresilient plastic
Curing MechanismSolvent Evaporation
Shelf Lifeindefinite
SolventMethylethylketone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNDIND14 / 54764

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.