MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Perkadox PF-MT40Z tert-Butyl monoperoxymaleate, paste, 40% in dibutyl maleate
Categories: Other Engineering Material

Material Notes: Perkadox PF-MT40Z is a 40% suspension which is used for room temperature curing of acrylic solid surface without yellow discoloration. It is used in combination with Accelerator CTAS for room temperature cure.

CAS number: 1931-62-0

EINECS/ELINCS No.: 217-691-1

Applications: Perkadox PF-MT40Z can be used as for the ambient temperature curing of MMA resins. Without the addition of an accelerator, the cure of the acrylate resin starts only above the activation temperature of 90°C. For the cure at ambient temperature, Perkadox PF-MT40Z must be accelerated with a combination of special accelerators. The most important advantage of a cure system based on Perkadox PF-MT40Z is the absence of yellow discoloration and a lower residual monomer content compared to results obtained with a BPO/amine curing system.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 188.2 g/mol
Storage Temperature <= 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 50.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 3.00 Month
 
Descriptive Properties
Assay38.0 - 42.0 %
Content (%)8.5Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY829 / 286352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.