MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox B Acrylics Di-tert-butyl peroxide
Categories: Other Engineering Material

Material Notes: Trigonox B is an initiator for (co)polymerization of acrylates and methacrylates.

CAS number: 110-05-4

EINECS/ELINCS No: 203-733-6

Applications: Polymer production: Polymerization of ethylene: Trigonox B is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes. In most cases a combination with other peroxides is used to ensure a broad reactivity range. For Crosslinking: Due to its high volatility, Trigonox B is mainly used for compounds that are crosslinked immediately after mixing. Trigonox B is a thermally relatively stable crosslinking peroxide. However, the high vapor pressure and the low flashpoint (+6°C) require special attention during handling and use. Trigonox B tends to build up static electricity; pumps must be ignition proof with grounded stainless steel tubing. Avoid any exposure to heat from naked fire, sunlight, steam pipes or any other source during storage. Safe processing temperature: 145°C (rheometer ts2 > 20 minutes). Typical crosslinking temperature: 180°C (rheometer t90 about 12 minutes).

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.800 g/cc0.0289 lb/in³
Half-life  0.100
@Temperature 164 °C
0.100
@Temperature 327 °F
[hr]
 1.00
@Temperature 141 °C
1.00
@Temperature 286 °F
[hr]
 10.0
@Temperature 121 °C
10.0
@Temperature 250 °F
[hr]
Viscosity 0.90 cP0.90 cP
Molecular Weight 146.2 g/mol146.2 g/mol
Storage Temperature -30.0 - 40.0 °C-22.0 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 80.0 °C176 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay= 99.0 %
Color= 30 Pt-Co / APHA
Content= 0.10 %tert-Butyl hydroperoxide
 = 10.83 %Active oxygen
Content (%)10.94Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1156 / 286679

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.