MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: ME2592 is a natural, high molecular weight, medium density polyethylene for crosslinkable pipes with excellent flexibility. The compound is especially designed for electron beam irradiation crosslinking. The stabilization package is optimized for good processability, easy crosslinking as well as service at high temperatures.

Crosslinkable pipes based on ME2592 are recommended for floor heating, radiator connections and for domestic hot and cold water supply. Pipes made from ME2592 meet drinking water requirements and DIN 16 894 (MD-PEX pipes)

Former trade name for this product was BorPEX™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.936 g/ccBase Resin; ISO 1183
Oxidative Induction Time (OIT) >= 40 min210°C; EN 728/AI cup
High Load Melt Index 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3191 psiAt 50 mm/min; ISO 527
Elongation at Yield 10 %ISO 527-2
Tensile Modulus 0.840 GPaISO 527-2
Flexural Modulus 0.680 GPaAt 2 mm/min; ISO 178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
Borealis HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE1878E High Density Polyethylene Powder for Crosslinked Pipes

PBOREA025 / 27332

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.