MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
ITW Insulcast® RTVS 42 CURTIS II Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 42 CURTIS II is a low viscosity unique silicone-epoxy copolymer formulated to withstand severe thermal shock and provide low moisture absorption and excellent dielectric insulation. It is UL 94V-0 certified under file # E86165. RTVS 42 CURTIS II contains silane adhesion promoters that enable it to bond well to most metals and plastics. Its unique chemistry combines the low temperature performance characteristics heretofore found only in silicones with the excellent encapsulating properties of epoxies.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccUncured. Part B
 1.43 g/ccUncured. Part A
Viscosity 125 cPPart B; ASTM D1084
 16000 cPMixed, Part A, Part B; ASTM D1084
 18000 cPPart A; ASTM D1084
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75ASTM D2240
Hardness, Shore D 10 - 15
Tensile Strength 900 psiASTM D412
Elongation at Break 175 %ASTM D412
Tear Strength 40.0 pliDie B; ASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 4.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 500 V/milASTM D149
Dissipation Factor 0.0060
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
Thermal Conductivity 0.580 W/m-K
Maximum Service Temperature, Air 125 °C
 155 °Cintermittent use
Minimum Service Temperature, Air -55.0 °C
Glass Transition Temp, Tg -60.0 °Ccured
Flammability, UL94 V-0
Shrinkage 0.20 - 0.50 %
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
8 hrs @ 25°C plus 2 hours @ 65°C
 24.0 hour
@Temperature 25.0 °C
option
Pot Life <= 20.0 minPart A, Part B
Shelf Life 9.00 MonthPart A, Part B
 
Descriptive Properties
Coloramberpart B, uncured
 blackpart A, uncured
Mix Ratio by volume100:7Part A: Part B
Mix Ratio by weight100:4-8Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWIN9121 / 239631

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.