MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Graft Polymer GRAFTABOND™ SB-PU 01510 C Styrene-Butadiene Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: GRAFTABOND™ SB-MAH 01510 C is based on SBC matrix, with high amount of grafted isocyanate functional groups. Isocyanates offer compatibility with polyurethane, polyurethane compounds and polyamides. Supplied as: Granulate. Applications: GRAFTABOND™ SB-PU 01510 C functions as coupling agent and impact modifier between reinforcing materials (glass fibers, natural and inorganic fillers) and polyurethane matrices
  • Compatibility with polyamides, impact toughener of polyamide blends.

    Properties can be regulated to customer needs.

    Information provided by Graft Polymer LTD.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Melt Flow 13 - 18 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Descriptive Properties
    Drying Loss<0.5 %. ASTM D6980. 105°C
    Isocyanate Group Content0.5 to 1.3 %. FTIR

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Graft Polymer GRAFTABOND™ PPC-GMA 02030 C Polypropylene grafted with Glycidyl Methacrylate
    Graft Polymer GRAFTABOND™ SB-MAH 00220 C Styrene Butadiene Copolymer Grafted with Maleic Anhydride
    Graft Polymer GRAFTABOND™ UHP-MAH 00030 IM Highly functionalized Ultra High Molecular Weight Polyethylene with Maleic Anhydride
    Graft Polymer GRAFTABOND™ SB-MAH 03020 C Styrene Butadiene Copolymer Grafted with Maleic Anhydride
    Graft Polymer GRAFTABOND™ SB-GMA 00330 C Styrene Butadiene Copolymer Grafted with Glycidyl Methacrylate

    PGRAFT951 / 232382

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.