MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPE ME-2640DB Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2600 series are super high flow high performance thermoplastic elastomer series, available in BLK, designed for automotive exterior molded applications. Sarlink ME-2640DB is a high hardness, low density, UV stabilized, super high flow injection molding grade excellent delivering excellent aesthetics.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Good Processability; Good Surface Finish; Low Density; High Flow; Low Specific Gravity; High Hardness; UV Resistant

Uses: Automotive Applications; Automotive Exterior Part

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.941 g/cc0.0340 lb/in³ISO 1183
Viscosity 215 cP
@Shear Rate 206 1/s,
Temperature 200 °C
215 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
19 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  48
@Time 5.00 sec
48
@Time 0.00139 hour
ISO 868
 53
@Time 1.00 sec
53
@Time 0.000278 hour
ISO 868
Tensile Strength at Break 19.3 MPa2800 psiFlow; ISO 37
 22.8 MPa3310 psiAcross Flow; ISO 37
 21.4 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
3100 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 21.6 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
3130 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  10.4 MPa
@Strain 100 %
1510 psi
@Strain 100 %
Flow; ISO 37
 12.8 MPa
@Strain 100 %
1860 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 600 %600 %Flow; ISO 37
 780 %780 %Across Flow; ISO 37
 671 %
@Treatment Temp. 125 °C,
Time 605000 sec
671 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
 720 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
720 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
Tear Strength 82.4 kN/m470 pliFlow; ISO 34-1
 94.7 kN/m540 pliAcross Flow; ISO 34-1
Compression Set  44 %
@Temperature 22.8 °C,
Time 79200 sec
44 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 66 %
@Temperature 70.0 °C,
Time 79200 sec
66 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 77 %
@Temperature 90.0 °C,
Time 252000 sec
77 %
@Temperature 194 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 180 °C338 - 356 °F
Middle Barrel Temperature 180 - 200 °C356 - 392 °F
Front Barrel Temperature 200 - 250 °C392 - 482 °F
Nozzle Temperature 210 - 230 °C410 - 446 °F
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 10.0 - 60.0 °C50.0 - 140 °F
Injection Pressure 6.00 - 12.0 MPa870 - 1740 psi
Back Pressure 0.500 - 2.00 MPa72.5 - 290 psi
Screw Speed 50 - 120 rpm50 - 120 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1082 / 237573

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.