Product description: AUROmid® PA6 HGF10GB20 black Compound is a 10% glass fiber and 20% glass beads reinforced injection molding grade for dimensional stable, low distortion applications Typical applications: Housing parts, handles, switches Information provided by Aurora Kunststoffe GmbH |