MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC XYLEX™ X7519HP PC+Polyester (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend

Material Notes: Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts may form opaque areas in the centre due to slow cooling.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccISO 1183
Water Absorption 0.16 %23°C/sat; ISO 62
Moisture Absorption 0.140 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
 12.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 66.0 MPa50 mm/min; ISO 527
 66.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa50 mm/min; ASTM D638
 61.0 MPa50 mm/min; ISO 527
Elongation at Break 120 %50 mm/min; ASTM D638
 134 %50 mm/min; ISO 527
Elongation at Yield 2.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2370 MPa1mm/min; ISO 527
 2470 MPa5 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 98.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2030 MPa2 mm/min; ISO 178
 2240 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 700 J/mASTM D256
 100 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 13.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 74.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 112 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 113 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 130 °CRate B/50; ASTM D1525
 130 °CRate B/50; ISO 306
 132 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 °CHopper Temperature
Nozzle Temperature 280 - 290 °CInjection Molding
Zone 1 275 - 285 °C
Zone 2 280 - 290 °C
Zone 3 290 - 300 °C
Melt Temperature 280 - 300 °C
Mold Temperature 65.0 - 75.0 °C
Drying Temperature 85.0 - 100 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.100 - 0.500 MPa
Shot Size 40 - 80 %
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11640 / 245107

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.