MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® Nylene 2407 HSSP Specialty Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: High viscosity nylon copolymer with high impact resistance and superior flexibility. Optimized with good melt strength for high line speeds in thin wall sections, and is available in natural and black. 2407 HSSP is one of a family of grades specifically designed for the convoluted tubing industry, but can also be used for other extrusions and some molded parts.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccISO 1183
Melt Flow 3.0 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPaISO 527
Elongation at Break 300 %ISO 527
Tensile Modulus 900 MPaISO 527
Flexural Modulus 800 MPaISO 978
Izod Impact, Notched 20.0 J/mISO 180
 
Thermal PropertiesOriginal ValueComments
Melting Point 218 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 39.0 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 258P1 Black 2N PA 66, Dry
Domo TECHNYL® B 230 Grey 1429 H PA 66/6, Conditioned
Domo TECHNYL® B 230 Black-H PA 66/6, Conditioned
Envalior Arnitel® EL740 74 Shore D, Injection Grade Copolyester Elastomer (North America)
Envalior Arnitel® EL740 TPC-ET, Injection Molding

PNYLEN976 / 221508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.