MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nucrel™ 0403 Ethylene Methacrylic Acid
Categories: Polymer; Thermoplastic

Material Notes: Product Description: Nucrel™ 0403 is a copolymer of ethylene and methacrylic acid, made with nominally 4% methacrylic acid. The resin is available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.
Uses: Adhesives; Packaging; Sealants

Composition: 4% by weight Methacrylic Acid comonomer content

Availability: Africa 7 Middle East; Asia Pacific; Europe; Latin America; North America

Agency Ratings: FDA 21 CFR 177.1330 (a)

Form: Pellets

Processing Method: Blown Film; Cast Film; Coextrusion; Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
 0.932 g/cc0.0337 lb/in³ASTM D792
Melt Flow  3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °F
 110 °C230 °FPeak
Vicat Softening Point 95.0 °C203 °FASTM D1525
 95.0 °C203 °FISO 306
 
Descriptive Properties
Freezing Point198°FASTM D3418
 198°FISO 3146

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF552 / 311245

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.