Data provided by the manufacturer, Exxon Chemical. A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness. HDZ-123 is particularly recommended for films 0.5 mil or greater in thickness. Applications: Retail carry-out sacks; Merchandise bags; Institutional can liners; Consumer trash bags. Data for film properties below based on 0.5 mil film. |
High Density Polyethylene; Exxon Chemical Company |