MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP
Categories: Polymer; Adhesive

Material Notes: 3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints. The acrylic adhesive also provides excellent adhesion to surfaces contaminated lightly with oil typically used with machine parts. 3M™ Double Coated Tape 9496LE offers the added feature of 3M™ High Performance Acrylic Adhesive 200MP on one side to provide excellent bond strength to a variety of high surface energy substrates.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milFaceside Adhesive
 50.8 microns2.00 milCarrier
 50.8 microns2.00 milBackside Adhesive
 112 microns4.40 milCaliper
 170 microns6.70 milTotal Thickness
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.53686 kN/m3.0625 pliStainless Steel, 90°, 15 min RT, Faceside; ASTM D3330
 0.64642 kN/m3.6875 pliStainless Steel, 90°, 15 min RT, Backside; ASTM D3330
 0.833 kN/m4.75 pliStainless Steel, 90°, 72 hr RT, Backside; ASTM D3330
 0.97511 kN/m5.5625 pliStainless Steel, 90°, 72 hr RT, Faceside; ASTM D3330
 1.2161 kN/m6.9375 pliStainless Steel, 90°, 72 hr at 70°C, Faceside; ASTM D3330
 1.23 kN/m7.00 pliStainless Steel, 90°, 72 hr at 70°C, Backside; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FLong term
 149 °C300 °FShort term
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
AppearanceBackside
 Faceside
LinerTan, 58# Polycoated Kraft
 Tan, 58# Polycoated Kraft

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® 2302-3R UHMW Film Backing Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® 2253-2 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive
Resin Technology Group UV MX-2230 Quick Fixture, Activator Cured, One-Component, Acrylic Adhesive
Permabond TA430 Acrylic Adhesive & Initiator

PMM33277 / 168024

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.