MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parson Adhesives PARFIX® 3426 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3426 is high viscosity combined with medium cure speed, and excellent resistance to peel and shock loads. It is specifically formulated to bond various Rubbers, Metals and Plastics for use in challenging environments. PARFIX 3426 resists thermal shock and can be used in temperature up to 223 °F.

Applications:

  • Ideal for bonding Rubbers, Metals and Plastics.
  • Ideal for wide variety of Rubber and Metal bonding.
  • Slower cure speed for alignment of parts.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 lb/gal
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 870 psiPVC; ASTM D1002
 >= 1020 psiPolycarbonate; ASTM D1002
 >= 2030 psiSBR Rubber; ASTM D1002
 >= 2320 psiNeoprene Rubber; ASTM D1002
 >= 2470 psiAluminum; ASTM D1002
 >= 2610 psiNitrile Rubber; ASTM D1002
 1890 - 4210 psi
 >= 3480 psiSteel; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D696
Dielectric Constant 2.3ASTM D150
Dielectric Strength 25.0 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CASTM D696
Thermal Conductivity 0.100 W/m-KASTM C177
Melting Point 160 - 170 °C
Maximum Service Temperature, Air 80.0 °C
Minimum Service Temperature, Air -60.0 °F
Glass Transition Temp, Tg 120 °CASTM E228
Flash Point >= 93.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.200 - 0.367 minNeoprene Rubber, Fixture
 0.200 - 0.367 minNitrile Rubber, Fixture
 0.167 - 0.4167 minAluminum, Fixture
 0.250 - 0.4167 minSBR Rubber, Fixture
 0.330 - 0.4167 minPolyurethane, Fixture
 0.500 - 1.33 minPolycarbonate, Fixture
 0.830 - 1.50 minPVC, Fixture
 1.00 - 1.67 minSteel, Fixture
 24.0 hourFull
 
Descriptive Properties
AppearanceBlack Liquid
CompositionRubber Toughened Ethyl Cyanoacryalte
Gap Filling0.75 mm
Initial Strength Retained (%)75Gasoline for 1000 hrs at 22°C
 80Gasoline for 500 hrs at 22°C
 85Isopropanol for 500 hrs at 22°C
 85Isopropanol for 1000 hrs at 22°C
 90Motor Oil for 500 hrs at 40°C
 90Motor Oil for 1000 hrs at 40°C
 90Mineral Spirit for 500 hrs at 22°C
 90Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPARSN129 / 186572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.