MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ZEON Zetpol® ZLX 2230LX Latex Hydrogenated Nitrile Elastomer (HNBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Zetpol 2230LX is a hydrogenated carboxylated acrylonitrile/butadiene copolymer latex, medium-highly saturated with medium-high acrylonitrile content. Zetpol 2230LX is supplied as a light-gray liquid.

Zetpol® hydrogenated nitrile (HNBR) is a tough, durable elastomer. Zetpol resists prolonged exposure to 160°C and provides superior resistance to hot fluids. The toughness of Zetpol makes it the ideal choice for automotive belt, seals, and oil field components. Zetpol is classified as a DH-DK polymer according to SAE J200 / ASTM D200.

Information provided by Zeon Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40 - 41 %KY 239 / KY 745
pH 8.0 - 10Test 92B
Brookfield Viscosity <= 50 cP
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °C
 
Descriptive Properties
Bound Acrylonitrile (%)31.9R142C
 34.5R142C
Iodine Value28.0 mg/100mgMin. ZCI-T-004/NZ:R133
 44.0mg/100mgMax. ZCI-T-004/NZ:R133

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEON925 / 250105

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.