MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Michelman® Michem® Emulsion 93335 Nonionic polyethylene emulsion
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Nonionic polyethylene emulsion

Usage: Michem® Emulsion 93235 is a phenol free additive best used in water based coatings where improved slip, rub resistance, hardness and/or block resistance is needed. Michem® Emulsion 93235 has proven very effective for mar resistance in floor polish formulations as well as mar resistance and shine in car polish formulations.

We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foam

Food Contact Information when manufactured in USA:
FDA:
175.105: Components of adhesives.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 - 1.01 g/cc0.990 - 1.01 g/cc
Volatiles 64.5 - 65.5 %64.5 - 65.5 %
pH >= 7.0>= 7.0Recommended pH of system
 9.0 - 109.0 - 10
Brookfield Viscosity <= 50 cP<= 50 cPSpindle # 1, rpm 60
 
Descriptive Properties
AppearanceTranslucent liquid
Emulsifier ChargeNonionic
Solids TypeHigh Density Polyethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHEL112 / 135029

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.