Notes: Telcar TELC 340-S is a general purpose thermoplastic elastomer, available in NAT and BLK, designed for the automotive and industrial market. Telcar TELC 340-S is a high hardness, low density, unfilled grade suitable for injection molding, blow molding and extrusion. Features: High Hardness; Low Density; Low Flow; Low Specific Gravity; Without Fillers Uses: Automotive Applications; Blow Molding Applications; General Purpose; Grommets; Industrial Applications; Weatherstripping Automotive Specifications: CHRYSLER MS-DC-243 Color: Natural; CHRYSLER MS-DC-243 CPN 2705, 2390 Color: Black Form: Pellets Processing Method: Extrusion; Injection Molding Information Provided by Teknor Apex |