MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Elvax® 3130SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: 12 wt% Vinyl Acetate.

General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent drawability for easy processing, good flex-crack resistance for liquid packaging, high toughness, low shrink for water bath applications, and excellent optical properties. It adheres to many materials. It is commonly used as a tie layer in certain coextrusions with dissimilar surfaces.

Information provided by DuPont Packaging Polymers.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/ccASTM D792
Moisture Vapor Transmission 0.870 cc-mm/m²-24hr-atmg-mm/m²-day; based on 1 mil (0.0254 mm) thick film; ASTM E96
Oxygen Transmission 225 cc-mm/m²-24hr-atm
@Thickness 0.0254 mm
Based on 1 mil (0.0254 mm) thick film; ASTM D3985
Melt Flow 2.5 g/10 minCondition not noted.; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 520 %MD-TD Average; ASTM D882
Film Elongation at Break, TD 520 %MD-TD Average; ASTM D882
Impact 23.6J/mm Spencer Impact; Average of MD and TD; ASTM D3420
Elmendorf Tear Strength, MD 71.0 g/milAverage of MD and TD; ASTM D1922
Film Tensile Strength at Break, MD 22.8 MPaMD-TD Average; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 76.0 °CFreezing Point via DSC/ASTM D3418
 95.0 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 72.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 25 %ASTM D1003
Gloss 47 %20°; ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Elvax® 3165Z Ethylene Vinyl Acetate
DuPont Elvax® 3136 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
DuPont Elvax® 3135B Ethylene Vinyl Acetate
DuPont Elvax® 3134Q Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating, Casting
DuPont Elvax® 3130SBZ Ethylene-Vinyl Acetate Copolymer Resin for Blown Film

PDUPH6 / 33609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.