MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECASINT 2391 black Polyimide, 15% MoS2 Filled
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Machined, MoS2 Filled

Material Notes:
  • high thermal and mechanical capacity
  • very good slide and wear properties
  • low outgassing
  • very good thermal stability
  • good chemical resistance
  • high creep resistance
  • resistance against high energy radiation
  • sensitive to hydrolysis in higher thermal range
Target Industries:
  • aircraft and aerospace technology
  • cryogenic engineering
  • precision engineering
  • vacuum technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³
Water Absorption  0.53 %
@Temperature 23.0 °C,
Time 86400 sec
0.53 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
 1.58 %
@Temperature 80.0 °C,
Time 86400 sec
1.58 %
@Temperature 176 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8888DIN EN ISO 868
Ball Indentation Hardness 265 MPa38400 psiISO 2039-1
Tensile Strength 95.0 MPa13800 psi50 mm/min; DIN EN ISO 527-1
Elongation at Break 3.5 %3.5 %50 mm/min; DIN EN ISO 527-1
 4.0 %4.0 %10 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 4.41 GPa640 ksi1 mm/min; DIN EN ISO 527-1
Flexural Strength 140 MPa20300 psi10 mm/min; DIN EN ISO 178
Flexural Modulus 3.90 GPa566 ksi2 mm/min; DIN EN ISO 178
Compressive Strain at Break 35.6 %35.6 %10 mm/min; EN ISO 604
Compressive Yield Strength 165 MPa
@Strain 10 %
23900 psi
@Strain 10 %
10 mm/min; EN ISO 604
Compressive Strength 230 MPa33400 psi10 mm/min; EN ISO 604
Compressive Modulus 2.00 GPa290 ksi1 mm/min; EN ISO 604
 
Thermal PropertiesMetricEnglishComments
CTE, linear  40.0 µm/m-°C
@Temperature 50.0 - 200 °C
22.2 µin/in-°F
@Temperature 122 - 392 °F
XY; DIN 53 752
 47.0 µm/m-°C
@Temperature 50.0 - 200 °C
26.1 µin/in-°F
@Temperature 122 - 392 °F
Z; DIN 53 752
 50.0 µm/m-°C
@Temperature 200 - 300 °C
27.8 µin/in-°F
@Temperature 392 - 572 °F
XY; DIN 53 752
 57.0 µm/m-°C
@Temperature 200 - 300 °C
31.7 µin/in-°F
@Temperature 392 - 572 °F
Z; DIN 53 752
Glass Transition Temp, Tg 357 °C675 °F
Flammability, UL94 V-0V-0DIN IEC 60695-11-10
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8200 / 319128

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.