MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Okulen® 2000 PE-UHMW, AB
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistatic finish and additional lubricant for the conveyor industry. With added antioxidants, for example, which can be used at high temperatures. With additional flame retardant properties for use in rail vehicle, machinery and mining construction. With enhanced antibacterial effects.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccISO 1183-A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ISO 868
Tensile Strength, Yield >= 17.0 MPaISO/R 527
Elongation at Break >= 50 %ISO/R 527
Creep Strength 10.0 MPa
Coefficient of Friction, Dynamic 0.13
@Pressure 2.00 MPa
PE-metal, V = 10 m/min; ASTM D1894
Coefficient of Friction, Static 0.18
@Pressure 2.00 MPa
PE-metal, V = 10 m/min; ASTM D1894
Abrasion 80Slurry-Test rel to GUR 4120 = 100%; DIN 58836
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+14 ohm-cmTeil 30; IEC 600093 / VDE 0303
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°CDIN 53752
Melting Point 135 - 137 °CISO 3146
Maximum Service Temperature, Air 80.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow EP-9289 LL Cosmetic Powder
Silon Taborex TA 1108 HD Chemically-Crosslinkable HDPE Compound
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)

POKUL027 / 83469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.