MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Silpak RU-448 Performance Polyurethane Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: RU-448 A/B is a 45 shore A hardness, polyurethane RTV elastomer that cures to a rubber material with excellent tear strength and abrasion resistance. It has a simple 1:1 mix ratio and low viscosity for easy processing.

Features:

  • Excellent tear resistance and elongation
  • Easy to process
  • Rapid mold cycle
Applications: Applications include the following or any application where a flexible rubber part is required:
  • Concrete texture and stamp pads
  • Rubber molds and parts
  • Concrete form liners
  • Prototype rubber parts

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Viscosity 3000 cP3000 cPInitial Mixed
Storage Temperature 17.8 - 30.0 °C64.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545
Tensile Strength 4.48 MPa650 psi
Elongation at Break 800 %800 %
Tear Strength 15.8 kN/m90.0 pli
 
Processing PropertiesMetricEnglishComments
Cure Time 960 min
@Temperature 22.8 °C
16.0 hour
@Temperature 73.0 °F
Demold
Gel Time 30.0 min30.0 min
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorYellow
Mix Ratio1A:1Bby weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSILPAK007 / 318644

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.