MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: High Flow High Gloss, Fancy Applications

Information provided by Bhansali

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.045 g/cc0.03775 lb/in³ASTM D-792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D-955
Melt Flow 55 g/10 min
@Load 10.0 kg,
Temperature 220 °C
55 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 113113ASTM D-785
Tensile Strength, Yield 43.1 MPa
@Thickness 3.20 mm
6260 psi
@Thickness 0.126 in
Type 1; ASTM D-638
Flexural Yield Strength 62.8 MPa
@Thickness 6.40 mm
9100 psi
@Thickness 0.252 in
ASTM D-790
Flexural Modulus 2.21 GPa
@Thickness 6.40 mm
320 ksi
@Thickness 0.252 in
ASTM D-790
Izod Impact, Notched  0.980 J/cm
@Thickness 6.40 mm
1.84 ft-lb/in
@Thickness 0.252 in
ASTM D-256
 1.1765 J/cm
@Thickness 3.20 mm
2.2041 ft-lb/in
@Thickness 0.126 in
ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °FMethod A - Annealed; ASTM D-648
Vicat Softening Point 103 °C217 °FMethod B; ASTM D-1525
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
UL-94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade
Bhansali Engineering Abstron SHF-50+M ABS Injection Molding Grade
Edinburg Plastics AGG625 ABS
Edinburg Plastics AGG645 ABS
Bhansali Engineering Abstron MIF45EP ABS Injection Molding Grade

PBHANS01 / 27110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.