Crossvinil: PVC compound modify with NBR that have good resistance to oil Crossvinil ME/8 P: it present good deformation and compression resistance and have a good resistance properties to flex-fatigue and to abrasion. Also good resistance to the fuels. They conserve their flexibility and elasticity in a big range of temperatures. Certify: ENI 018100 Information provided by Crosspolimeri S.P.A. |