Notes: Telcar TL-1017A is a high performance thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. Telcar TL-1017A is a low density, high hardness, lubricated grade that is RoHS complaint. This grade suitable for both injection molding and extrusion. Features: Bromine Free; Good Colorability; Good Melt Strength; Good Mold Release; Good Moldability; Good Processability; Good Processing Stability; Good Tear Strength; Halogen Free; High Hardness; High Melt Stability; High Tensile Strength; Light Stabilized; Low Density; Low Flow; Low Specific Gravity; Lubricated; Without Fillers Uses: Insulation; Jacketing; Wire & Cable Applications; Wire Jacketing Form: Pellets Processing Method: Injection Molding; Extrusion Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpm Information Provided by Teknor Apex |