MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraiburg TPE THERMOLAST® K TF8ADN Thermoplastic Elastomer (FC/AD1/PS Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FC/AD1/PS series is a material solution for applications of daily life with regulatory requirements. It is characterized by its adhesion to polar thermoplastics such as ABS, PC, PC/ABS and PS. The natural colored materials can be colored in many different ways.

Processing Method: Injection Molding, Extrusion

Color / RAL DESIGN:

  • Natural
Typical applications:
  • Toys
  • Grip applications
  • Household articles
  • Razors
  • Function and design elements
  • Toothbrushes
  • Soft touch surface (thumb wheels, push buttons, switches)
  • Bumpers
Material advantages:
  • Adhesion to PC, ABS, PC/ABS, ASA, SAN
  • Adhesion to PET and PETG
  • Adhesion to PS
  • Soft, velvety feel
  • Halogen-free (according to IEC 61249-2-21)
  • Colorable

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³DIN EN ISO 1183-1
Spiral Flow 25.0 cm
@Pressure 76.0 MPa,
Temperature 200 °C
9.84 in
@Pressure 11000 psi,
Temperature 392 °F
DSOP Lab 2032
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777DIN ISO 48-4
Tensile Strength 8.00 MPa1160 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 700 %700 %200 mm/min; DIN 53504/ISO 37
Tear Strength 29.0 kN/m165 pliISO 34-1 Method B (b)
 
Descriptive Properties
Adhesion to ABS5.0 N/mm (A)VDI 2019 two-component injection
Adhesion to PC6.0 N/mm (A)VDI 2019 two-component injection
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8173 / 308837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.