MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QGel 324 General Purpose Silicone Gel
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QGel 324 is a clear, very soft, moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.

Key Features:

  • One to one mix ratio
  • Soft, but resilient gel
  • Dispensing equipment not necessary
  • Excellent self-healing properties, which is an optimal choice for connectors

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccUncatalyzed A
 0.970 g/ccUncatalyzed B
Viscosity 3000 cPUncatalyzed A
 3000 cPUncatalyzed B
 
Mechanical PropertiesOriginal ValueComments
Penetration 4.0 - 9.0
@Temperature 150 °C,
Time 1800 sec
[mm], Cured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
 20.0 min
@Temperature 150 °C
 60.0 min
@Temperature 100 °C
Gel Time 180 minCatalyzed
 
Descriptive Properties
ColorTransparentUncatalyzed A
 TransparentUncatalyzed B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CHT Group QGel 319 Optically Clear Silicone Gel
CRG Industries Essemplex AB43 Thermoplastic Shape Memory Polymer Resin
CRG Industries Essemplex AF34 Thermoplastic Shape Memory Polymer Resin
SpinTech Veritex™ Shape Memory Polymer Composite
CHT Group QGel 326 General Purpose Silicone Gel

PACC2024 / 199412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.