MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman DuraStar DS1900HF Polymer, Natural
Categories: Polymer; Thermoplastic; Polyester, TP; Polycyclohexylenedimethylene Terephthalate (PCT); Glycol-Modified PCT (PCTG) Copolyester

Material Notes: Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding features of Durastar are easily maintained such as excellent appearance and clarity, good physical properties, chemical resistance, and easy processing. This high flow product is especially suited for those applications utilizing thin-walled intricate tools. Under existing United States Food and Drug Administration (FDA) regulations, Durastar DS1900HF may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.

Applications/Uses

  • Appliances
  • Furniture/Furniture trim
  • Toys/Sporting goods
  • Floor care
  • Housewares
  • Writing instruments
  • Key Attributes

  • Good chemical resistance
  • Excellent flow
  • Outstanding impact resistance
  • Excellent clarity
  • Fast drying times
  • Quick cycle times

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Specific Gravity 1.19 g/ccASTM D792
    Water Absorption 0.15 %24h Immersion; ASTM D570
    Linear Mold Shrinkage 0.0030 cm/cmASTM D955
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell R 107ASTM D785
    Tensile Strength at Break 43.0 MPaASTM D638
    Tensile Strength, Yield 50.0 MPaASTM D638
    Elongation at Break 270 %ASTM D638
    Elongation at Yield 5.0 %ASTM D638
    Flexural Yield Strength 68.0 MPaASTM D790
    Flexural Modulus 1.90 GPaASTM D790
    Izod Impact, Notched 0.440 J/cm
    @Temperature -40.0 °C
    ASTM D256
     80.0 J/m
    @Temperature 23.0 °C
    ASTM D256
    Izod Impact, Unnotched NBASTM D4812
     NB
    @Temperature -40.0 °C
    ASTM D4812
    Puncture Energy 40.0 JPuncture Resistance @Max Load, 23°C; ASTM D3763
     38.0 J
    @Temperature -40.0 °C
    Puncture Resistance at Max Load; ASTM D3763
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 73.0 °CASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CASTM D648
    Vicat Softening Point 86.0 °C1kg load; ASTM D1525
     
    Optical PropertiesOriginal ValueComments
    Haze <= 1.0 %ASTM D1003
    Transmission, Visible 92 %Total Transmittance; ASTM D1003
     
    Processing PropertiesOriginal ValueComments
    Melt Temperature 230 - 280 °C
    Mold Temperature 15.0 - 30.0 °C
    Drying Temperature 70.0 °C
    Dry Time 4 hour
     
    Compliance PropertiesOriginal ValueComments
    FDA YesSee notes for details.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Eastman DuraStar DS1000 Polymer, Natural
    Eastman Eastar MN211 Copolyester, Natural
    Eastman DuraStar DS2000 Polymer, Natural
    Eastman DuraStar DS1910HF Polymer, Natural
    Eastman DuraStar DS1110UVI Polymer, Natural

    PE9007 / 35063

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.