MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon® PFA Grade 940 HP Plus Extrusion and Molding Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: DuPont™ Teflon® PFA HP Plus fluoropolymer is a special purpose resin available in clear, 2.5-mm (0.1 in) pellets. This resin is similar to PFA HP with the additional benefits of improved flex life and chemical stress crack resistance. Teflon® PFA HP Plus meets the increasingly stringent requirements for ultra-reliable and non-contaminating parts, while retaining the same exceptional chemical resistance, high purity and protection against ionic contamination as PFA HP. The improved flex life and chemical resistance will reduce the cost of ownership of high purity fluid handling systems by reducing downtime caused by mechanical or chemical stresses. Parts molded with Teflon® PFA HP Plus have improved clarity and a smooth finish, which can further help prevent buildup of microbial contamination in water handling systems.

The exceptional purity of Teflon® PFA HP Plus makes it suitable for applications that require low extractable fluorides, and freedom from other foreign materials. This product contains no additives and is designed for hostile chemical environments where purity in the parts-per-billion range is needed. An example is in fluid handling systems for the manufacture of semiconductors. Teflon® PFA HP Plus is preferred when extended service is required in hostile environments involving chemical, thermal, and mechanical stress. Table 1 shows the typical property data for Teflon® PFA HP Plus.

The excellent thermal stability of Teflon® PFA HP Plus results in better moldings and reduces metal pickup from processing equipment. Teflon® PFA HP Plus combines the processing ease of conventional thermoplastics with the properties similar to those of polytetrafluoroethylene.

Properly processed products made from Teflon® PFA HP Plus resin provide the superior properties typical of fluoropolymer resins; retention of properties after service at 250°C (482°F), useful properties at –196°C (–320°F), and chemical inertness to nearly all industrial chemicals and solvents. Dielectric properties are excellent. Molded products have moderate stiffness and high ultimate elongation.

In a flame situation, products of Teflon® PFA HP Plus resist ignition and do not themselves promote flame spread. When ignited by flame from other sources, their contribution to heat is very small and added at a slow rate with very little smoke.

Applications

Applications for Teflon® PFA HP Plus include tubing; pipe, fittings, valves, and other components for ultrapure fluid handling systems, either unsupported or for linings.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.12 - 2.17 g/cc2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.050 %<= 0.050 %24 hours; ASTM D570
Melt Flow 14 - 19 g/10 min14 - 19 g/10 minASTM D3307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength, Ultimate 28.0 MPa4060 psiASTM D3307
 11.0 MPa
@Temperature 200 °C
1600 psi
@Temperature 392 °F
ASTM D3307
Tensile Strength, Yield 14.0 MPa2030 psiASTM D3307
Elongation at Break 310 %310 %ASTM D3307
 450 %
@Temperature 200 °C
450 %
@Temperature 392 °F
ASTM D3307
Flexural Modulus 0.650 GPa94.3 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant 2.02 - 2.08
@Frequency 100 - 1.00e+7 Hz
2.02 - 2.08
@Frequency 100 - 1.00e+7 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.0250 mm
2030 kV/in
@Thickness 0.000984 in
film; ASTM D149
Dissipation Factor <= 0.00030
@Frequency 100 - 1.00e+7 Hz
<= 0.00030
@Frequency 100 - 1.00e+7 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear  150 µm/m-°C
@Temperature 21.0 - 100 °C
83.3 µin/in-°F
@Temperature 69.8 - 212 °F
ASTM D696
 230 µm/m-°C
@Temperature 100 - 149 °C
128 µin/in-°F
@Temperature 212 - 300 °F
ASTM D696
 290 µm/m-°C
@Temperature 149 - 208 °C
161 µin/in-°F
@Temperature 300 - 406 °F
ASTMD 696
Melting Point 285 - 300 °C545 - 572 °FASTM D3418
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 379 - 399 °C714 - 750 °FCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm1800000
Heat of Combustion J/g5300ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours1000
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance10Years unaffected in Florida Exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Chemours Teflon® PFA Grade 345 Extrusion and Molding Resin
Bakelite® PF 1141 Phenolic Formaldehyde Resin, High Surface Quality, Resistant to High Temperatures, Dishwasher Proof
Chemours Teflon® PFA Grade 345T Extrusion and Molding Resin for High Temperature Applications
Overview of materials for Polyetheretherketone, Unreinforced

PDU9224 / 33337

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.