MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion Vit 106a Zirconium-Based Bulk Metallic Glass (BMG)  (discontinued **)
Categories: Metal; Nonferrous Metal; Zirconium Alloy

Material Notes: BMGs (amorphous alloys formed by rapid cooling) have strength-to-weight ratios more than twice those of titanium, magnesium and aluminum alloys. Amorphous alloys typically have elastic limits that can be three times higher than crystalline metallic alloys and exhibit outstanding corrosion resistance due to their atomic structure and composition.

Information supplied by Materion.

Key Words: Liquidmetal™ designation LM106a
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1800 MPa
Modulus of Elasticity 95.0 GPa
Fracture Toughness 30.0 MPa-m½
 
Thermal PropertiesOriginal ValueComments
Melting Point 837 °C
Crystallization Temperature 499 °C
Glass Transition Temp, Tg 395 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 3.65 %
Copper, Cu 13 %
Nickel, Ni 9.9 %
Niobium, Nb (Columbium, Cb) 3.4 %
Zirconium, Zr 70 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion Vit 105 Zirconium-Based Bulk Metallic Glass (BMG)
Materion Vit 1b Zirconium-Based Bulk Metallic Glass (BMG)
Materion Vit 601 Zirconium-Based Bulk Metallic Glass (BMG)
NanoAmor 90% Regular Single Walled Carbon Nanotubes
Goodfellow Zirconium 56.5/Vanadium 43.5 Alloy

NBB953 / 192260

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.