MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC
Categories: Polymer; Thermoset; Composite SMC; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: LYTEX 4181 is an epoxy ESC molding compound designed for structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and low density. It utilizes a 12K Tow carbon fiber reinforcement.

  • Form = Sheet
  • Color = Black
  • Glass Fiber Content = 55%

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Linear Mold Shrinkage 0.00 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 206 MPaASTM D638
Flexural Strength 413 MPaASTM D790
Flexural Modulus 31.0 GPaASTM D790
Izod Impact, Notched 800 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.450 W/m-K
Maximum Service Temperature, Air >= 260 °CDeflection Temperature, Load not specified; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 265 - 330 °FMold Temperature
Cure Time 5.00 - 10.0 min
Shelf Life 6.00 Month
@Temperature -12.2 °C
 
Descriptive Properties
Fiber Length (in)1Carbon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites LYTEX® 4182 50-55% Carbon Fiber Reinforced Epoxy SMC
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Epoxy Novolac 27%, Carbon fabric 73%
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC

PCOQB915 / 139283

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.