MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.35 - 1.76 g/ccAverage value: 1.58 g/cc Grade Count:87
Filler Content 25.0 - 30.0 %Average value: 27.4 % Grade Count:21
Water Absorption 0.0700 - 1.26 %Average value: 0.459 % Grade Count:33
Moisture Absorption at Equilibrium 0.150 - 0.300 %Average value: 0.190 % Grade Count:13
Water Absorption at Saturation 0.200 - 0.900 %Average value: 0.704 % Grade Count:13
Additive Loading 25.0 - 30.0 %Average value: 26.7 % Grade Count:3
Maximum Moisture Content 0.200 - 0.200
@Temperature 100 - 100 °C
Average value: 0.200 Grade Count:1
 0.200 - 0.200
@Time 299 - 299 sec
Average value: 0.200 Grade Count:1
Linear Mold Shrinkage 0.00100 - 0.0220 cm/cmAverage value: 0.00591 cm/cm Grade Count:61
Linear Mold Shrinkage, Transverse 0.00800 - 0.0205 cm/cmAverage value: 0.0123 cm/cm Grade Count:21
Melt Flow 0.300 - 16.0 g/10 minAverage value: 6.48 g/10 min Grade Count:38
Ash 22.0 - 28.0 %Average value: 25.0 % Grade Count:4
 23.0 - 27.0 %
@Temperature 625 - 625 °C
Average value: 25.0 % Grade Count:1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80.0 - 101Average value: 89.3 Grade Count:14
Hardness, Rockwell R 84.0 - 122Average value: 103 Grade Count:11
Ball Indentation Hardness 175 - 239 MPaAverage value: 203 MPa Grade Count:9
Tensile Strength, Ultimate 50.0 - 182 MPaAverage value: 116 MPa Grade Count:64
 45.0 - 158.579 MPa
@Temperature -40.0 - 120 °C
Average value: 75.1 MPa Grade Count:3
Tensile Strength, Yield 14.0 - 137 MPaAverage value: 83.4 MPa Grade Count:26
 26.2001 - 159.269 MPa
@Temperature -40.0 - 120 °C
Average value: 89.0 MPa Grade Count:3
Elongation at Break 1.00 - 13.0 %Average value: 3.29 % Grade Count:74
 4.00 - 5.80 %
@Temperature 60.0 - 90.0 °C
Average value: 4.90 % Grade Count:1
Elongation at Yield 2.00 - 9.00 %Average value: 4.56 % Grade Count:9
Modulus of Elasticity 3.70 - 12.0 GPaAverage value: 8.23 GPa Grade Count:55
 2.50 - 8.10 GPa
@Temperature 40.0 - 140 °C
Average value: 5.10 GPa Grade Count:2
Flexural Yield Strength 75.8 - 285 MPaAverage value: 169 MPa Grade Count:61
Flexural Modulus 3.24 - 10.9 GPaAverage value: 7.42 GPa Grade Count:70
 3.44738 - 5.70 GPa
@Temperature 60.0 - 120 °C
Average value: 4.45 GPa Grade Count:2
Izod Impact, Notched 0.374 - 5.34 J/cmAverage value: 0.804 J/cm Grade Count:44
 0.37373 - 0.550 J/cm
@Temperature -40.0 - 82.2 °C
Average value: 0.447 J/cm Grade Count:4
Izod Impact, Unnotched 2.67 - 6.94 J/cmAverage value: 5.02 J/cm Grade Count:15
Izod Impact, Notched (ISO) 2.60 - 9.00 kJ/m²Average value: 6.37 kJ/m² Grade Count:15
 6.00 - 9.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 7.50 kJ/m² Grade Count:2
Charpy Impact Unnotched 1.80 - 7.00 J/cm²Average value: 3.94 J/cm² Grade Count:19
 1.80 - 6.00 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 3.79 J/cm² Grade Count:8
Charpy Impact, Notched 0.240 - 4.10 J/cm²Average value: 0.876 J/cm² Grade Count:41
 0.220 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.613 J/cm² Grade Count:9
Coefficient of Friction 0.370 - 0.600Average value: 0.485 Grade Count:3
Tensile Creep Modulus, 1 hour 3300 - 8500 MPaAverage value: 5700 MPa Grade Count:4
Tensile Creep Modulus, 1000 hours 2100 - 6000 MPaAverage value: 4280 MPa Grade Count:5
K (wear) Factor 300 - 10000 x 10-8 mm³/N-MAverage value: 4590 x 10-8 mm³/N-M Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10000 - 1.00e+16 ohm-cmAverage value: 1.10e+15 ohm-cm Grade Count:43
Surface Resistance 1.00e+6 - 5.00e+16 ohmAverage value: 6.47e+15 ohm Grade Count:32
Dielectric Constant 3.70 - 5.00Average value: 4.26 Grade Count:13
Dielectric Strength 17.7 - 43.0 kV/mmAverage value: 26.8 kV/mm Grade Count:26
Dissipation Factor 0.00300 - 0.0300Average value: 0.00985 Grade Count:12
Comparative Tracking Index 500 - 600 VAverage value: 593 V Grade Count:14
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.8 - 90.0 µm/m-°CAverage value: 44.0 µm/m-°C Grade Count:27
CTE, linear, Transverse to Flow 60.0 - 125 µm/m-°CAverage value: 96.4 µm/m-°C Grade Count:17
Specific Heat Capacity 1.20 - 1.81 J/g-°CAverage value: 1.38 J/g-°C Grade Count:7
Thermal Conductivity 0.215 - 0.470 W/m-KAverage value: 0.303 W/m-K Grade Count:3
Melting Point 165 - 203 °CAverage value: 168 °C Grade Count:42
Maximum Service Temperature, Air 85.0 - 140 °CAverage value: 112 °C Grade Count:10
Deflection Temperature at 0.46 MPa (66 psi) 145 - 177 °CAverage value: 165 °C Grade Count:29
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 180 °CAverage value: 156 °C Grade Count:70
Vicat Softening Point 150 - 162 °CAverage value: 158 °C Grade Count:12
Flammability, UL94 HBGrade Count:47
Flame Spread 40.0 - 49.0 mm/minAverage value: 44.3 mm/min Grade Count:3
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 230 °CAverage value: 164 °C Grade Count:29
Nozzle Temperature 180 - 220 °CAverage value: 198 °C Grade Count:6
Die Temperature 190 - 210 °CAverage value: 199 °C Grade Count:13
Melt Temperature 160 - 230 °CAverage value: 193 °C Grade Count:44
Mold Temperature 40.0 - 130 °CAverage value: 88.7 °C Grade Count:44
Injection Velocity 20.0 - 50.0 mm/secAverage value: 35.0 mm/sec Grade Count:4
Drying Temperature 79.4 - 121 °CAverage value: 98.1 °C Grade Count:45
Moisture Content 0.150 - 0.200 %Average value: 0.157 % Grade Count:20
Dew Point -31.7 °CAverage value: -31.7 °C Grade Count:8
Injection Pressure 30.0 - 140 MPaAverage value: 86.2 MPa Grade Count:33

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acetal Copolymer, Unreinforced
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
Overview of materials for Nylon 66, 40% Glass Fiber Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled

O1253 / 77842

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.