Product description: Grilon FG 40 NL natural 6021 is a modified, high viscosity polyamide 6. As a result of the modification in comparison to conventional polyamide 6 Grilon FG40 NL natural 6021 offers the following improvements:- Better gas barrier properties at elevated humidity and after pasteurization and sterilization
- Better optical and UV- barrier properties
- Better aroma barrier and flavor protection
- Better thermoforming and orientation properties
Application examples: Grilon FG 40 NL natural 6021 is suitable for the manufacture of mono and coextruded blown and castfilms. Grilon FG 40 NL natural 6021 is used as oriented films, sausage casings and deepdrawn films as packaging for meat cheese, fish (pouches, shells, covers)at elevated humidity levels.Information provided by EMS Grivory. |