MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC NORYL GTX™ Resin GTX674PC Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 674PC resin is a conductive, non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for in- or on-line primer-less powder coat painting around corners and holes with a Class A Surface. NORYL GTX674PC resin exhibits high heat resistance, improved surface appearance and is an excellent candidate for automotive applications such as mirror housings and brackets. This material is only available in black.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Heat Stabilized,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
Moisture Absorption 0.0700 %0.0700 %Injection Molding
Linear Mold Shrinkage, Flow 0.010 - 0.013 cm/cm
@Thickness 3.20 mm
0.010 - 0.013 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 300 °C
25 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psi50 mm/min; ISO 527
 64.0 MPa9280 psi50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ASTM D638
Elongation at Break 4.0 %4.0 %50 mm/min; ASTM D638
 4.0 %4.0 %50 mm/min; ISO 527
Elongation at Yield 3.0 %3.0 %50 mm/min; ASTM D638
 3.0 %3.0 %50 mm/min; ISO 527
Tensile Modulus 2.81 GPa408 ksi5 mm/min; ASTM D638
Flexural Strength 103 MPa14900 psiyield, 2 mm/min; ISO 178
 109 MPa15800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.48 GPa360 ksi2 mm/min; ISO 178
 2.89 GPa419 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 74.0 J54.6 ft-lbASTM D256
 50.0 J
@Temperature -30.0 °C
36.9 ft-lb
@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 4.00 J2.95 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1000 - 10000 ohm-cm1000 - 10000 ohm-cmSABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  76.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
42.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 81.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
45.0 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 86.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
47.8 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 185 °C365 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 188 °C
@Thickness 3.20 mm
370 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 196 °C385 °FRate B/120; ISO 306
 197 °C387 °FRate B/50; ASTM D1525
 197 °C387 °FRate B/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 280 - 305 °C536 - 581 °F
Zone 2 270 - 305 °C518 - 581 °F
Zone 3 275 - 305 °C527 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 75.0 - 120 °C167 - 248 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82128 / 290075

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.