MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BEC Materials SBS 792E
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Description: As an environmentally friendly non-oil-extended rubber, SBS rubber 792E doesn't contain any nonylphenol. Thermoplastic elastomer SBS rubber is polystyrene(S)-polybutadiene(B)-polystyrene(S) triblock copolymer with linear molecular structure and medium molecular weight.

Application: Adhesives/Asphalt modification/Compounding

Formula: Shoe Adhesive (Parts by mass)
SBS(YH792E): 100
Coumarone Resin: 70-90
Terpene Resin:40-60
Antioxygen: 1
Gasoline and Ethyl Acetate: 450-500

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Viscosity 850 - 1850 cP850 - 1850 cPSolution, 25%
Melt Flow 0.10 - 5.0 g/10 min0.10 - 5.0 g/10 min
Ash <= 0.20 %<= 0.20 %
 
Chemical PropertiesMetricEnglishComments
Styrene Content 40 %40 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 85>= 85
Tensile Strength >= 24.0 MPa>= 3480 psi
Elongation at Break >= 700 %>= 700 %
300% Modulus >= 3.50 MPa>= 508 psi
 
Descriptive Properties
Oil Content0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBECM055 / 307008

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.