MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Sil-X® NLGI 1 Grease
Categories: Fluid; Lubricant; Silica Gellant

Material Notes: Features

Chevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.

It is transparent red in color, and has a smooth consistency with distinct stringiness.

Chevron Sil-X Grease provides outstanding lubrication in industrial applications where extremely high temperatures are encountered. The dropping points of Chevron Sil-X Grease exceeds 260°C (500°F). Chevron Sil-X Grease has a very high film strength and performs well under shock load conditions. It minimizes wear and prevents scuffing.

Its high viscosity oil and high viscosity additive characteristics enable this lubricant to seal bearings and resist leakage and washout.

Under high temperature operating conditions, the "no melt" silica keeps the lubricant in place long after conventional multipurpose greases would have melted and run out of bearings.

Chevron Sil-X Grease has an excellent pumpability characteristic.

Applications

Chevron Sil-X Grease is recommended for industrial applications subjected to very high temperatures requiring a lubricant which will not melt.

Typical applications are plain or journal bearings, antifriction bearings, gear cases in kiln cars, conveyors in ceramic and paint baking ovens furnace doors, shafts extending through furnaces, etc.

Key Words: CPS Number: 255779; MSDS Number: 6704
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9494Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 2506 SUS2506 SUS
Saybolt Viscosity at 210°F 150 SUS150 SUS
Kinematic Viscosity at 40°C (104°F) 467 cSt467 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 30.5 cSt30.5 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Penetration 325325Worked
Penetration P(0), 1/10 mm 328328
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -9.00 °C15.8 °F
Pour Point -12.0 °C10.4 °FASTM D97
Flash Point 304 °C579 °FASTM D92
 
Descriptive Properties
ColorRed
Lincoln Ventmeter, psig at 30 s, at 30°F200
Lincoln Ventmeter, psig at 30 s, at 75°F175
TextureSmooth
Thickener, % / type6 / Silica

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV267 / 74882

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.