MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici Raditeck® P RCM651K 1700 NT Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: PPS 65% glass fiber and mineral filler reinforced injection. Lubricated, easier processing. Heat stabilized. Natural color.

Balanced matching of excellent chemical resistance, inherent flame retardancy and very good heat aging properties retention. Suitable for parts requiring high stiffness and high mechanical strength, along with good dimensional stability and low warp age. Ease of processing thanks to good flow ability.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.93 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 315 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa5mm / min.; ISO 527-2/1A
Elongation at Break 0.70 %5 mm / min.; ISO 527-2/1A
Tensile Modulus 23150 MPa1mm / min.; ISO 527-2/1A
Flexural Strength 205 MPa2mm / min.; ISO 178
Flexural Modulus 23500 MPa2mm / min.; ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²ISO 180/1A
Charpy Impact Unnotched 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 150 VSol.A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.7 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 31.5 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 280 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 275 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 260 °CISO 75/2Af
Flammability, UL94 V-0
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 300 - 340 °CInjection Molding
Mold Temperature 140 - 160 °C
 
Descriptive Properties
Injection Molding Injection SpeedLow- medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6990 / 293495

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.