MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Vinnapas® UW 4 FS Vinyl Acetate Homopolymer
Categories: Polymer; Thermoplastic

Material Notes: VINNAPAS® UW 4 FS is a solid, thermoplastic homopolymer. The clear and colorless resin is prepared by polymerization of vinyl acetate. VINNAPAS® UW 4 FS is tasteless.

Application: Typical applications for VINNAPAS® UW 4 FS:

  • fiber reinforced plastics
  • Adhesives
  • powder injection molding
  • sound damping

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 - 0.850 g/ccDIN 53466
Density 1.18 g/ccDIN EN ISO 2811/1-3
Volatiles <= 1.0 %
Viscosity 23 - 30 cP10% in ethylacetate; ASTM D445-06
Brookfield Viscosity >= 740 cP20 rpm, 20% solid content in styrene
 >= 7100 cP20 rpm, 30% solid content in styrene
 >= 66000 cP20 rpm, 40% solid content in styrene
Molecular Weight 280000 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.50[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 155 °CRing and Ball; DIN ISO 4625
Glass Transition Temp, Tg 44.0 °CDIN EN ISO 11357-2
 
Descriptive Properties
K-Value60-66DIN 53726

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Intex® 2740 Styrene - Butadiene Copolymer
Applied Nanotech Ag-iJ10 Silver Ink
Applied Nanotech Cu-iJ70P Copper Ink
Versalis Europrene Latice® 5570 Styrene - Butadiene Copolymer
Versalis Europrene Latice® 5577 Styrene - Butadiene Copolymer

PWACK9659 / 205188

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.