Kaocrete 28-LI is a general-purpose, low iron monolithic which contains an intermediate-purity calcium aluminate cement that can be cast or gunned into place. Designed for applications up to 2800°F (1538°C), Kaocrete 28-LI a economical choice for high-temperature applications. Features: Recommended use limit up to 3000°F (1649°C) Aggregate chemistry and grain sizing High purity binder systems Installed by cast, gun or plaster Applications: Around water-cooled boiler tubesBoiler ash hoppersKiln carsPiersCar bottomsSeal tanks in FCCU vessels Burner blocksLadle metallurgy lance materialInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |