MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade

Processing and Delivery Form: Pellets and Injection Molding

Additives: Glass fiber

Special Characteristics: Autoclavable, dimensional stability, high temp resistant

Information provided by Oxford Polymers

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ASTM D792
Water Absorption at Saturation 0.25 %0.25 %ASTM D570
Linear Mold Shrinkage, Flow 0.0055 cm/cm
@Thickness 3.17 mm
0.0055 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 159 MPa23000 psiASTM D638
Elongation at Break 3.8 %3.8 %ASTM D638
Flexural Strength 239 MPa34600 psiASTM D790
Flexural Modulus 7.58 GPa1100 ksiASTM D790
Izod Impact, Notched 1.49 J/cm
@Thickness 3.17 mm
2.80 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 343 °C650 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 360 °C680 °F
Middle Barrel Temperature 371 °C700 °F
Front Barrel Temperature 374 °C705 °F
Nozzle Temperature 379 °C715 °F
Melt Temperature 363 °C685 °F
Mold Temperature 177 °C350 °F
Drying Temperature <= 149 °C<= 300 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2202 HF  Polyetheretherketone (PEEK) Glass Fiber 15% - High Flow
RTP Company RTP 2201.3 LF  Polyetheretherketone (PEEK) Glass Fiber 13% - Low Flow
RTP Company RTP 2200.5 LF  Polyetheretherketone (PEEK) Glass Fiber 5% - Low Flow
Oxford Polymers PEEK-20CF-Black PEEK, 20% Carbon Fiber Reinforced
Overview of materials for Polyphenylsulfone (PPSU)

POXF012 / 178442

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.