MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Very good corrosion resistance, weldable, and resistant to sensitization.

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4571; ASTM 316Ti; JIS SUS 316Ti
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 165Outokumpu Typical, 20°C, Hot rolled plate (Quarto)/Cold rolled strip/sheet; EN 10003-1
Tensile Strength, Ultimate 570 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 360 MPa
@Temperature 500 °C
EN min.; EN 10002-5
 375 MPa
@Temperature 300 °C
EN min.; EN 10002-5
 375 MPa
@Temperature 400 °C
EN min.; EN 10002-5
 390 MPa
@Temperature 200 °C
EN min.; EN 10002-5
 440 MPa
@Temperature 100 °C
EN min.; EN 10002-5
 840 MPa
@Temperature -80.0 °C
EN min; EN 10002-5
 1200 MPa
@Temperature -196 °C
EN min; EN 10002-5
Tensile Strength, Yield 220 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 270 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 310 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 129 MPa
@Strain 0.2 %,
Temperature 500 °C
EN min.; EN 10002-5
 135 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 145 MPa
@Strain 0.2 %,
Temperature 300 °C
EN min.; EN 10002-5
 158 MPa
@Strain 1 %,
Temperature 500 °C
EN min.; EN 10002-5
 164 MPa
@Strain 1 %,
Temperature 400 °C
EN min.; EN 10002-5
 167 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 175 MPa
@Strain 1 %,
Temperature 300 °C
EN min.; EN 10002-5
 185 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
 196 MPa
@Strain 1 %,
Temperature 200 °C
EN min.; EN 10002-5
 218 MPa
@Strain 1 %,
Temperature 100 °C
EN min.; EN 10002-5
 275 MPa
@Strain 0.2 %,
Temperature -80.0 °C
EN min.; EN 10002-5
 350 MPa
@Strain 0.2 %,
Temperature -196 °C
EN min.; EN 10002-5
 355 MPa
@Strain 1 %,
Temperature -80.0 °C
EN min.; EN 10002-5
 450 MPa
@Strain 1 %,
Temperature -196 °C
EN min.; EN 10002-5
Elongation at Break 50 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 35 %
@Temperature -196 °C
EN min
 40 %
@Temperature -80.0 °C
EN min
Modulus of Elasticity 200 GPaRT
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 300 °C
 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
Poissons Ratio 0.30RT
Shear Modulus 77.0 GPacalculated
Impact Test >= 60.0 JHot rolled plate/Cold rolled strip/sheet, 10x10mm test pieces; EN 10045-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000750 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 100 °C
 17.5 µm/m-°C
@Temperature 200 °C
 18.0 µm/m-°C
@Temperature 300 °C
 18.5 µm/m-°C
@Temperature 400 °C
 19.0 µm/m-°C
@Temperature 500 °C
Specific Heat Capacity 0.500 J/g-°CRT
Thermal Conductivity 15.0 W/m-KRT
 20.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %
Chromium, Cr 16.8 %
Iron, Fe 70.16 %
Molybdenum, Mo 2.1 %
Nickel, Ni 10.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel
Crucible Steel 431 Chromium Steel
316 Stainless Steel, annealed bar
Schmolz + Bickenbach UGICHROM 4057 Martensitic Chrome Plated Bar
ATI Allegheny Ludlum 316Ti Austenitic Stainless Steel

NOUTOK27 / 18742

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.