MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LD 6520.BA Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: ExxonMobil™ LD 6520.BA is a homopolymer, garment film resin with good toughness. It is capable of being drawn-down to thin gauges.

Availability: North America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: No
Applications:
  • Blown Film
  • Cast Film
  • Compounding
  • Garment Film
  • Hygiene Film
  • Laundry Film

Information provided by ExxonMobil

Key Words: LDPE LGA 105
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccExxonMobil method
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 9.00 lb (f)
Film Tensile Strength at Yield, MD 1400 psiASTM D882
Film Tensile Strength at Yield, TD 1400 psiASTM D882
Film Elongation at Break, MD 420 %ASTM D882
Film Elongation at Break, TD 670 %ASTM D882
Puncture Energy 13.0 in-lbExxonMobil Method
 13.0 in-lb
Elmendorf Tear Strength MD 530 gASTM D1922
Elmendorf Tear Strength TD 210 gASTM D1922
Dart Drop Test 80.0 gASTM D1709A
Film Tensile Strength at Break, MD 3400 psiASTM D882
Film Tensile Strength at Break, TD 2700 psiASTM D882
1% Secant Modulus, MD 25000 psiASTM D882
1% Secant Modulus, TD 30000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 231 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 86.0 °C
 
Optical PropertiesOriginal ValueComments
Haze 5.7 %ASTM D1003
Gloss 75 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force8 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman PE1059 Film Extrusion Polyethylene
Huntsman PE5050 Extrusion Coating Polyethylene
Westlake EC472 Low Density Polyethylene
LyondellBasell Lupolen 2421K Low Density Polyethylene (LDPE), Film Grade
LyondellBasell Lupolen 2420K Low Density Polyethylene (LDPE), Film Grade

PEX99238 / 175474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.