MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® Nylene 401F Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Food-contact FDA compliant un-reinforced nylon 6 injection molding resin. High flow characteristics at minimal processing temperatures. Suitable for applications in both thin and heavy sections that require typical nylon characteristics and easy molding. Compliant with 21CFR177.1500.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 79.3 MPa11500 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Modulus 2.69 GPa390 ksiASTM D790
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 182 °C360 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °C309 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
BASF Ultramid® A34 01 PA66 (Dry)
BASF Ultramid® A27 E 01 PA66 (Dry)
Avient Trilliant™ HC HC6620-0033 RS Natural Polyamide 66 (Nylon 66)

PNYLEN909 / 221441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.