MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ohara S-LAL12 Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes: ECO optical glass that does not contain any lead or arsenic.

Information provided by Ohara Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 4.01 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 53
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 560
@Load 0.0999 kg
Modulus of Elasticity 91.0 GPa
Modulus of Rigidity 35.4 GPa
Poissons Ratio 0.284
Abrasion 166Aa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.20 µm/m-°C
@Temperature -30.0 - 70.0 °C
 8.60 µm/m-°C
@Temperature 100 - 300 °C
Thermal Conductivity 0.717 W/m-K
@Temperature 35.0 °C
Transformation Temperature, Tg 652 °Cper thermal expansion curve
Softening Point 716 °C107.65 poise; JIS-R3104 and ASTM-C338
Annealing Point 630 °C1013 poise; ASTM-C336
Strain Point 604 °C1014.5 poise; JIS-R3103 and ASTM-C336
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64414
@Wavelength 2325.42 nm
 1.65021
@Wavelength 1970.09 nm
 1.65669
@Wavelength 1529.58 nm
 1.66242
@Wavelength 1128.64 nm
 1.66433
@Wavelength 1013.98 nm
nt (Hg t line)
 1.66768
@Wavelength 852.11 nm
ns (Cs s line)
 1.66998
@Wavelength 768.19 nm
nA' (K A' line)
 1.67208
@Wavelength 706.52 nm
nr (He r line)
 1.67419
@Wavelength 656.27 nm
nC (H C line)
 1.67478
@Wavelength 643.85 nm
nC' (Cd C' line)
 1.67533
@Wavelength 632.8 nm
nHe-Ne
 1.67779
@Wavelength 589.29 nm
nD (Na D line)
 1.67790
@Wavelength 587.56 nm
nd (He D line)
 1.68082
@Wavelength 546.07 nm
ne (Hg e line)
 1.68644
@Wavelength 486.13 nm
nf (H F line)
 1.68714
@Wavelength 479.99 nm
nF' (Cd F' line)
 1.69225
@Wavelength 441.57 nm
nHe-Cd
 1.69314
@Wavelength 435.835 nm
ng (Hg g line)
 1.69872
@Wavelength 404.656 nm
nh (Hg h line)
 1.70826
@Wavelength 365.015 nm
ni (Hg i line)
Abbe Number 55.08ν e
 55.34ν d
Optical Dispersion 0.003712nd-nC; Partial Dispersion
 0.004212nC-nA'; Partial Dispersion
 0.00558nh-ng; Partial Dispersion
 0.006042ne-nC'; Partial Dispersion
 0.006319nF'-ne; Partial Dispersion
 0.006632ne-nC; Partial Dispersion
 0.006703ng-nF; Partial Dispersion
 0.009855nC-nt; Partial Dispersion
 0.010445nC'-nt; Partial Dispersion
 0.01225nF-nC
 0.012361nF'-nC'
 0.015119ni-ng; Partial Dispersion
 0.015241ng-nd; Partial Dispersion
 0.021121ni-nF'; Partial Dispersion
Transmission, Visible 97.6 %
@Wavelength 380 nm
 98.4 %
@Wavelength 390 nm
 98.8 %
@Wavelength 400 nm
 99.2 %
@Wavelength 420 nm
 99.4 %
@Wavelength 440 nm
 99.5 %
@Wavelength 460 nm
 99.7 %
@Wavelength 480 nm
 99.8 %
@Wavelength 500 nm
 99.8 %
@Wavelength 600 nm
 99.8 %
@Wavelength 650 nm
 99.8 %
@Wavelength 700 nm
 99.9 %
@Wavelength 550 nm
IR Transmittance 73 %
@Wavelength 2400 nm
 90.1 %
@Wavelength 2200 nm
 98.1 %
@Wavelength 1800 nm
 99.1 %
@Wavelength 1400 nm
 99.1 %
@Wavelength 1600 nm
 99.6 %
@Wavelength 1000 nm
 99.6 %
@Wavelength 1200 nm
 99.7 %
@Wavelength 900 nm
 99.9 %
@Wavelength 800 nm
UV Transmittance 6.0 %
@Wavelength 280 nm
 15 %
@Wavelength 290 nm
 29 %
@Wavelength 300 nm
 45 %
@Wavelength 310 nm
 61 %
@Wavelength 320 nm
 73 %
@Wavelength 330 nm
 83 %
@Wavelength 340 nm
 89 %
@Wavelength 350 nm
 93.8 %
@Wavelength 360 nm
 96.2 %
@Wavelength 370 nm
 
Descriptive Properties
Acid Resistance, Powder Method, RAP)5
CCI0.00 B
 0.26 G
 0.26 R
coloring, λ 5285
coloring, λ 80360
Coloring, Internal Transmission λ 0.05279
Coloring, Internal Transmission λ 0.80337
Knoop Hardness Class6
Melt Frequency2
Ohara Code d678553
Ohara Code e681551
Ohara StatusPreferred
Phosphate Resistance, PR4.2
Photoelastic Constant (ß)1.61
Relative Price4S-BSL7 = 1
Water Resistance, RW(P)3
Weathering Resistance (Surface Method) W(S)max2
Yield Point, At (°C)679per thermal expansion curve

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ohara L-LAL12 Low Tg Optical Glass
Schott N-SF11 Glass
Schott SF11 785258.474, Optical Glass
Schott N-SK2HT 607567.355, Optical Glass
Schott N-LAK12 Glass

CZOHARA897 / 192162

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.